MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Dow Affinity™ PL 1888G Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: Affinity PL 1888G R Polyolefin Plastomer for Packaging films is used for high speed packaging applications requiring low seal initiation temperature and good machinablity (low consistent coefficient of friction and low block force). This resin is designed to five a COF of <0.2 for an ~1.0 mil sealant layer in a coextruded film and run fast and trouble-free on most extrusion equipment, including blown film dies equipped with narrow die gaps.
  • For use in monolayer films and as the sealant layer in multilayer films
  • For fresh-cut produce, meat, cheese and other high speed packaging applications requiring good machinability
  • Fast processing on narrow die gaps
Complies with: US FDA FCN 424; EU No 10/2011. Consult the regulations for complete details.

Availability: Latin America; North America

Additive: Antiblock: 3000 ppm; Processing Aid: Yes; Slip: 1500 ppm

Form: Pellets

Processing Method: Blown Film; Cast Film

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Antiblock Level
  • Slip Level
  • Puncture Resistance
  • Film Tensile Strength at Yield, MD, ASTM D882
  • Film Tensile Strength at Yield, TD, ASTM D882
  • Film Elongation at Break, MD, ASTM D882
  • Film Elongation at Break, TD, ASTM D882
  • 2% Secant Modulus, ASTM D882, TD
  • 2% Secant Modulus, ASTM D882, MD
  • Puncture Energy
  • Coefficient of Friction, Dynamic, ASTM D1894, vs. Itself
  • Elmendorf Tear Strength MD, ASTM D1922, 0.002
  • Elmendorf Tear Strength TD, ASTM D1922, 0.002
  • Dart Drop Test, ASTM D1709B
  • Film Tensile Strength at Break, MD, ASTM D882
  • Film Tensile Strength at Break, TD, ASTM D882
  • Heat Seal Strength Initiation Temperature, ASTM D1525
  • Melting Point
  • Vicat Softening Point, ASTM D1525
  • Haze, ASTM D1003
  • Gloss, ASTM D2457, 20°
  • Melt Temperature, Extrusion
  • Blow-up Ratio (BUR)
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.