MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
CMT Materials REN Shape® 5169 Foundry Pattern Board
Categories: Polymer

Material Notes: REN SHAPE 5169 is an extremely tough, abrasion resistant board for use in CNC-machining foundry patterns, core boxes and other tools. It can be milled with hardened-steel cutters. The material has found extensive use in the fabrication of prototype molds for clear, thin-gage thermoplastic sheets. Resultant parts show excellent transparency results. REN SHAPE 5169 features these unique qualities:

  • Excellent Impact and Wear Resistance
  • Superior Edge Definition and Dimensional Stability
  • Polishable to a High Luster
  • Good Compressive and Tensile Strength
  • Tough and Resilient

Applications: REN SHAPE 5169 applications may include prototype thermoforming molds, prototype and production foundry patters, tooling aids and fixtures, and metal forming tools.

Information Provided by CMT Materials, Inc.

Key Words: Renshape
Vendors:
Available Properties
  • Density, ASTM D-792
  • Hardness, Shore D, ASTM D-2240
  • Tensile Strength, Ultimate, ASTM D-638
  • Flexural Strength, ASTM D-790
  • Flexural Modulus, ASTM D-790
  • Compressive Strength, ASTM D-695
  • Compressive Modulus, ASTM D-695
  • Izod Impact, Notched
  • CTE, linear, ASTM D-3386
  • Glass Transition Temp, Tg, ASTM D-4065
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.