Maximum See-Through Clarity, Minimal Haze; Superior Color Stability, Process Stability, and Gloss; Low Odor, High Melt Flow Market Segment: Consumer Products and Cups & Containers Suggested Uses: Reusable Food Containers, Housewares, Fast-Cycle Injection Molding, Packaging Ultraclear™ polypropylene resin offers unsurpassed clarity and performance, up to 50% improvement in haze over standard clarified products. It offers substitution opportunities versus more expensive resins such as PET, PVC, PC or PS. Braskem acquired Sunoco Chemicals polypropylene product line in 2010. |