MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
A. Schulman Premi-Ject® 1101H-15 Polyester BMC  (discontinued **)
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Premi-Ject® 1101H-15 is a 15% fiberglass reinforced Bulk Molding Compound designed for applications requiring excellent impact strength, arc resistance, track resistance, dimensional stability, and flexural properties. Key features and benefits are:
  • Underwriters Laboratory, UL 94-HB flame recognition at 1.47mm minimum wall thickness.
  • UL recognized in all colors. Standard color is black.
  • Available in 10- 25% fiberglass content. Standard fiberglass content is 20 %.
  • Formulated to provide high mechanical properties and excellent electrical characteristics.
  • Designed for Compression, Transfer and Injection molding processes.

Data provided by Premix.

A. Schulman has acquired this former Premix product line.

Key Words: Bulk Molding Compound
Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Linear Mold Shrinkage, Ambient part /mold
  • Tensile Strength, Ultimate, ASTM D638
  • Modulus of Elasticity, ASTM D638
  • Flexural Yield Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Yield Strength, ASTM D695
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D4812
  • Dielectric Strength, ASTM D149
  • Arc Resistance, ASTM D495
  • Comparative Tracking Index, ASTM D3638
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
A. Schulman (Premix)

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.