MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Syensqo (Solvay Specialty Polymers) Solef® PVDF AM Filament MSC NT 1
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® PVDF AM Filament MSC NT 1 provides long term performance up to 120°C, including exceptional chemical resistance and outstanding UV, weathering and oxidation resistance. The product is also intrinsically endowed of a very high purity. These features make it particularly suited for outdoor applications, and applications in contact with harsh chemical environments, such as Chemical Processing Industry, Semiconductor Industry and Oil & Gas.

Applications: Additive Manufacturing (3D Printing); Industrial Applications; Oil/Gas Applications; Plumbing Parts

Features: Chemical Resistant; Flame Retardant; Good Weather Resistance; High Purity; Oxidation Resistant; UV Resistant

Printing conditions for data table:
- Filament drying conditions: drying not needed
- Extruder temperature: 225 - 235°C
- Bed temperature: 100°C
- Printing tool path: cross hatching in the XY plane

Test specimen parameters:
- Layer thickness: 0.2 mm
- 100% infill
- 3 shells
- Printing speed: 25 mm/s

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density
  • Tensile Strength at Break, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Melting Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.