MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Nouryon Armostat 1800 Octadecyl-bis(2-hydroxyethyl) amine
Categories: Other Engineering Material

Material Notes: Semi-permanent, vegetable-based alternative for Armostat 600, suitable for applications needing higher processing temperatures.

Applications: Armostat 1800 is a vegetable based saturated alkyl(C16-C18)bis(2-hydroxyethyl)amine. Armostat 1800 is an internal antistatic additive that can be used in various polymers such as PE, LLDPE, PP, SAN and ABS. Armostat 1800 gives sustained antistatic action and has due to its saturated alkyl chain excellent thermal stability. This makes Armostat 1800 especially suitable for those applications needing higher processing temperatures. Armostat 1800 is a solid at ambient temperatures. When heated at 60-65°C Armostat 1800 can be dosed as a liquid directly into the polymer by using a single or twin-screw extruder. Pigment or color concentrates should be mixed with the antistatic agent prior to extruding. Premixing ensures uniform distribution of Armostat 1800 in the resin while Armostat 1800 acts as a dispersion aid to the pigment color concentrate.

CAS number: 10213-78-2

EINECS/ELINCS No.: 233-520-3

Information provided by Nouryon

Vendors:
Available Properties
  • Density
  • Vapor Pressure
  • Flash Point, Cleveland open cup
  • H2O, Water
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.