MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ExxonMobil Label-Lyte™ 70LS447 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A two-side coated, shrink resistant, white, polypropylene film designed for use in hot melt cut-and stack labeling. It has an static resistant, matte finish, paper like print surface that is litho-printable, as well as compatible with water-based or solvent-based flexo and gravure inks and UV-cured inks. This film is deigned to be used as a monoweb and provides excellent converting performance, including printing, sheeting, guillotine cutting, and label transfer on magazine-fed labelers. The other side has a hot melt receptive coating.

Availability: Latin America, North America and South America

Key Features:

  • Excellent offset litho printing performance
  • Excellent static resistant properties for cut-and-stack labeling
  • Durable and moisture resistant
  • Excellent stiffness and burst performance
Features:
  • Static Resistant Coated
  • Static Resistant Matte Coated
Applications:
  • Beverage, Alcoholic
  • Beverage, Carbonated
  • Beverage, Mineral Waters
  • Dairy Products
  • Dry Foods and Beverage Powders
  • Household and Detergents
  • Industrial
Uses:
  • Cut & Stack (Hot Melt) Labels
Processing Method: Conventional Offset Lithography Printing, Digital Offset (HP Indigo) Printing, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported, Thermal Transfer Printing, UV Flexographic Printing, UV Screen Printing and Water-based Flexographic Printing

Information provided by ExxonMobil

Vendors:
Available Properties
  • Thickness, ExxonMobil Method
  • Coating Weight, ExxonMobil Method
  • Film Elongation at Break, MD, ExxonMobil Method, 20 in/min, 2.0 in Jaw Separation
  • Film Elongation at Break, TD, ExxonMobil Method, 20 in/min, 2.0 in Jaw Separation
  • Film Tensile Strength at Break, MD, ExxonMobil Method, 20 in/min, 2.0 in Jaw Separation
  • Film Tensile Strength at Break, TD, ExxonMobil Method, 20 in/min, 2.0 in Jaw Separation
  • Shrinkage, MD, ExxonMobil Method
  • Shrinkage, TD, ExxonMobil Method
  • Gloss, ExxonMobil Method, 45°, Print Surface
  • Transmission, Visible, ExxonMobil Method
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Exxon Chemical

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.