MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
KLJ Group KANATOL 400 I Plasticizer
Categories: Fluid

Material Notes: Properties: DIBP is almost colourless, odorless or slight aromatic, ester odor oily liquid, free of foreign materials..

Application: It is an excellent low cost plasticizer for cellulose nitrate. It resembles DBP but has a lower specific gravity and lower freezing point. DIBP is used effectively in protective coatings based on cellulose acetate, ethyl cellulose, vinyl polymers etc. DIBP is an effective plasticizer for polyvinyl acetate emulsion paints and its versatility is one of the prime benefit offered by it in the processing and applications of nitrite rubbers. Under the food and Additives Regulations , DIBP may lawfully be used in food packaging as an adhesive constituent. In manufacturing of footwear & hose pipes.

Chemical Name: DI Iso Butyl Phthalate

Molecular Formula: C 16 H22 O4

Molecular Structure: C 6 H 4 CO 2 [CH 2CH(CH 2) 2

CAS Number: 84-69-5

UN. NO: 3082

EINECS NO.: 201-553-2

Information provided by KLJ Group

Vendors:
Available Properties
  • Specific Gravity, ASTM D1045-08
  • Viscosity, KLJ TM-P-13-97
  • Molecular Weight
  • Boiling Point, IS 5298-05
  • Flash Point
  • Refractive Index, ASTM D1045-08
  • Moisture Content, ASTM E203-08
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.