Fluoroelastomer Rubber, 66-75 °IRHD. Terpolymer of vinylidene difluoride and hexafluoropropylene tetrafluoroethylene. Compounded to have extremely low temperature capability, Glass transition temperature -40 °C. Dependant on application, use temperature can be lower than this. Applications: Mouldings which are required to operate within the approximate temperature range of -40° and below to +225°C, in contact with air, petroleum, silicone and diester-based liquids. The material is not suitable for use in contact with certain phosphate-ester-based liquids. |