MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-820 SL45 PEEK, Very good wear resistance
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Very good wear resistance, lubricated, injection molding

KetaSpire® KT-820 SL45 is a PEEK based compound specifically designed to provide exceptionally low wear rates and good mechanical properties in applications where an external lubricant is provided.

Markets/Uses: Automotive / Air Induction / Air Pump Impeller; Automotive / Drivetrain / Lubricated; Automotive / Drivetrain / Seal Rings; Automotive / Drivetrain / Thrust Washers; Automotive / Mechanical & Structural Parts / Gears; Oil & Gas / Down Hole / Bushings and Bearings; Wear-Resistant Plastics / High Temperature Friction & Wear / Bearings; Wear-Resistant Plastics / High Temperature Friction & Wear / Gears; Wear-Resistant Plastics / High Temperature Friction & Wear / Lubricated

Applications: Automotive Applications; Bushings; Gears; Oil/Gas Applications; Thrust Washer

Features: Chemical Resistant; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; High Heat Resistance; Wear Resistant

Injection notes: Back Pressure: minimum

Information provided by Solvay Specialty Polymers.

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Viscosity, ASTM D3835, Melt
  • Linear Mold Shrinkage, Flow, ASTM D955
  • Linear Mold Shrinkage, Transverse, ASTM D955
  • Melt Flow, ASTM D1238
  • Hardness, Rockwell M, ASTM D785
  • Tensile Strength, ASTM D638
  • Tensile Strength, Yield, ISO 527-2, Type 1A, 5 mm/min
  • Elongation at Break, ASTM D638, 5.0 mm/min
  • Elongation at Break, ISO 527-2, Type 1A, 5 mm/min
  • Tensile Modulus, ASTM D638
  • Tensile Modulus, ISO 527-2, 1 mm/min, Type 1A
  • Flexural Strength, ASTM D790
  • Flexural Strength, ISO 178
  • Flexural Modulus, ASTM D790
  • Flexural Modulus, ISO 178
  • Compressive Strength, ASTM D695
  • Shear Strength, ASTM D732
  • Izod Impact, Notched, ASTM D256
  • Izod Impact, Unnotched, ASTM D256
  • Izod Impact, Notched (ISO), ISO 180
  • Izod Impact, Unnotched (ISO), ISO 180
  • CTE, linear, Parallel to Flow, ASTM E831
  • Specific Heat Capacity, ASTM C351
  • Specific Heat Capacity, ASTM C351
  • Thermal Conductivity, ASTM C177
  • Melting Point, ASTM D3418, Peak
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648, Annealed
  • Glass Transition Temp, Tg, DSC
  • Rear Barrel Temperature
  • Middle Barrel Temperature
  • Front Barrel Temperature
  • Nozzle Temperature
  • Mold Temperature
  • Drying Temperature
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay Specialty Polymers (includes former Solexis)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.