MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Daikin DAI-EL® G-801 Fluoroelastomer Terpolymer, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-801 is a peroxide curable copolymer with medium Mooney viscosity suitable for transfer and compression molding. DAI-EL® G-801can be formulated with various peroxide cure systems to eliminate the need for post cure. DAI-EL® G-801 provides superior mechanical properties and resistance to steam and aqueous solvents compared with bisphenol cured fluoroelastomers. DAI-EL® G-801 may be used in compliance with 21 CFR 177.2600, Rubber articles intended for repeated use. Finished articles are required to comply with the end tests specified in 21 CFR 177.2600 (e) or (f), as applicable.

Typical Applications: O-Rings, gaskets, seals

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors:
Available Properties
  • Specific Gravity
  • Mooney Viscosity, ML 1+10
  • Hardness, Shore A
  • Tensile Strength at Break
  • Tensile Strength at Break, Air Oven Aging
  • Elongation at Break
  • Elongation at Break, Air Oven Aging
  • 100% Modulus
  • Compression Set, ASTM D395 Method B, #214 O-ring
  • Compression Set, ASTM D395 Method B, #214 O-ring
  • Minimum Service Temperature, Air, Low Temperature Retraction, TR10
  • Minimum Service Temperature, Air, ASTM 1053-92A, Gehman Torsion T10
  • Minimum Service Temperature, Air, Low Temperature Retraction, TR70
  • Minimum Service Temperature, Air, ASTM 1053-92A, Gehman Torsion T2
  • Brittleness Temperature, Embrittlement
  • Cure Time, ts2, scorch time
  • Cure Time, t'50, time to 50% cure
  • Cure Time, t'90, time to 90% cure
  • Cure Time, Press Cure
  • Cure Time, Post cure
  • FDA, See notes for details.
  • Fluorine, F
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Daikin Industries

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.