MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Dow ENGAGE™ 11547 Polyolefin
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: Product Description: ENGAGE™ 11547 is a Polyolefin Elastomer offering very high flow and excellent rubber loading efficiency as superior impact modifier in thermoplastic polyolefin (TPO) compounds. Its improved toughening capability compared to other commercially available polyolefin elastomers allows for greater ease in optimizing elastomer levels to meet impact resistance requirements in global automotive specifications. TPO formulations containing ENGAGE™ 11547 combine very good processing behavior with very excellent stiffness/toughness balance for automotive parts, such as bumper fascia. The designed to ENGAGE™ 11547 polyolefin elastomer enables shorter injection molding cycle time for the TPO compound. Its designed characteristics contribute to morphology control and improved temperature resistance for final parts.
Main Characteristics:
  • High rubber loading efficiency for optimum cost/performance balance
  • Improved toughens for better stiffness/toughness balance
  • Very good flow characteristics
  • High crystallization temperature for short cycle time
  • High melting point for improved temperature resistance
  • Pellet form with partitioning agent for ease of handling
Applications:
  • Impact modification of TPO
  • Injection molded polyolefin compounds
Availability: Asia Pacific; Europe; Latin America; North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: EU No 10/2011; FDA FCN 424

Form: Pellets

Information provided by The Dow Chemical Company

Vendors:
Available Properties
  • Density, ASTM D792
  • Melt Flow, ASTM D1238
  • Hardness, Shore A, ASTM D2240, Compression Molded
  • Tensile Strength at Break, ASTM D638, Compression Molded
  • Elongation at Break, ASTM D638, Compression Molded
  • Tensile Modulus, ASTM D638, 100% Secant, Compression Molded
  • Tear Strength, ASTM D624
  • Melting Point
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Dow Chemical

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.