MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Borealis LE4217 Polyethylene Compound, Crosslinkable, Track Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE4217 is a black crosslinkable polyethylene compound designed for track resistant power cable insulation and jacketing. APPLICATION: LE4217 contains carbon black and UV stabilizer and specifically suited for outdoor installations such as OC cables. LE4217 is suitable as a jacket or insulation, for power cables rated up to 35kV. However it is recommended that for cables rated above 12kV, that a suitable conductor shield such as LE0594 or LE0595 be used for optimum performance. Specifications: ICEA S-94-649.

Information provided by Borealis AG

Key Words: XLPE
Vendors:
Available Properties
  • Density, ASTM D2839, base resin
  • Elongation at Break, ASTM D638, after aging 500h, 150°C
  • Elongation at Break, ASTM D2565, after xenon aging 2000h, 23°C
  • Elongation at Break, ASTM D638
  • Volume Resistivity, ASTM D257
  • Dielectric Breakdown, ASTM D2303, Tracking Resistance
  • Dissipation Factor, ASTM D150
  • Track Resistance, ASTM D2132
  • Melting Point
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.