MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Chesterton 850 Premium Sealing Tape
Categories: Polymer; Tape; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: Chesterton® 850 Premium Sealing Tape is a high density, moldable, dry PTFE thread sealing tape. It is a heavy duty, tear-resistant product containing more PTFE per inch than virtually any thread sealing tape on the market today. Chesterton 850 Premium Sealing Tape is chemically inert and seals most types of threaded metal and plastic pipes and bots. It is nonreactive with steam, water, air fuels, refrigerants, acids, alkalies, all solvents, and gases including hydrogen, oxygen, ammonia, propane, butane, and nitrogen. For nitric or mixed acid services, factory should be consulted. Chesterton 850 Premium Sealing Tape is non-hardening and stays pliable without the breakage seen in other PTFE containing tapes. It places a slippery layer of PTFE between mated threads which remains flexible and resists vibration. Connections that might otherwise be destroyed are saved for reuse as tape eases disassembly. Slippage is minimized during application as deep penetration for threads is possible with the soft malleable tape. Joints can be adjusted 90° or more without a leak. Chesterton 850 Premium Sealing Tape is packaged in rugged easy-to carry- spools which protect the tape of dirt and contamination

Features:

  • UL Listed - US Canada
  • Meets MIL-T-27730A
  • Meets USDA requirements for incidental food contact
  • Conforms to FDA21CFR 177.1615
  • Acceptable to oxygen use
  • Non-aging
  • Non-Hardening
  • High density
  • Chemically resistant

Benefits:

  • Stays pliable
  • Always ready to use
  • Requires fewer wraps
  • Resists tearing and breakage
  • Won't clog fuel lines.

Applications: Use Chesterton 850 Premium Sealing Tape as a non-hardening, dry thread sealant for most liquids, gases, pneumatic and hydraulic fittings. Prevents bolts and fittings from seize up to 260°C. Seals all plumbing and most industrial piping threads

Information provided by Chesterton

Vendors:
Available Properties
  • Specific Gravity
  • Thickness, ASTM D374
  • Tensile Strength at Break, ASTM D882, Longitudinal
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • FDA
  • USDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.