Temper: 1/4 Hard Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Brazing, Capacity for Being Cold Worked; Fair Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Spot Weld, Butt Weld; Poor Suitability – Capacity for Being Hot Formed Common Fabrication Processes: Blanking; Drawing; Machining; Piercing and Punching; Stamping Typical uses: Butts; Hardware; Hinge Brass; Trim; Watch Backs; Screw Machine Products Applicable Specifications: Bar – ASTM B121/B121M; Plate - ASTM B121/B121M; Rod, Bar & Shapes – ASTM B453/B453M; Sheet – ASTM B121/B121M; Strip – ASTM B121/B121M |