MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Film Properties.
  • Antiblock (2500 ppm)
  • Applications:

    • Industrial bags
    • Industrial packaging

    Film properties are typical of blown film extruded on a 2.5" extruder with 4" die and 35-mil die gap at a blow up ratio of 2.5:1, but are dependent upon operating conditions.

    United States: NOVAPOL TF-Y826-CP resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.2a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. NOVAPOL TF-Y826-CP resin is subject to the specific limitation that it may contact food only at temperatures of 212°F and below (21 CFR 176.170(c) Table 2, conditions of use B–H).

    NOVA Chemicals polyethylene resins are biologically and chemically inert.

    Key Words: Polyhexene; Polyolefin
    Vendors:
    Available Properties
    • Density, ASTM D792
    • Thickness
    • Melt Flow, ASTM D1238
    • Film Tensile Strength at Yield, MD, ASTM D882
    • Film Tensile Strength at Yield, TD, ASTM D882
    • Film Elongation at Break, MD, ASTM D882
    • Film Elongation at Break, TD, ASTM D882
    • Secant Modulus, MD, ASTM D882
    • Secant Modulus, TD, ASTM D882
    • Coefficient of Friction, ASTM D1894
    • Elmendorf Tear Strength, MD, ASTM D1922
    • Elmendorf Tear Strength, TD, ASTM D1922
    • Dart Drop, F 50; ASTM D1709/A
    • Film Tensile Strength at Break, MD, ASTM D882
    • Film Tensile Strength at Break, TD, ASTM D882
    • Haze, ASTM D1003
    • Gloss, 45°; 1 mil; ASTM D1894
    • Melt Temperature
    • FDA, See notes for details.
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    Manufacturer Notes:
    none

    Category Notes
    Plastic

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

     

    Rulon Bearings
    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.