MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Schmolz + Bickenbach 416 Stainless Steel Bar
Categories: Metal; Ferrous Metal; Martensitic; Stainless Steel; T 400 Series Stainless Steel

Material Notes: Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity, tool life and consistency, and improves the surface finish on all types of machined parts. Machined parts are frequently used in the annealed condition, but may be heat treated to develop optimum mechanical properties for specific applications. 416 HT, condition T (HRc26-32), is the popular heat-treated version of 416. This condition is specified for numerous engineering applications, and represents the optimum condition for both machinability and corrosion resistance. No further heat treatment of machined parts is required.

Hardened and tempered: Heat and hold 50°F to 100°F (10°C to 40°C) below tempering temperature for 4-7 hours, slow cool.

Information provided by Schmolz + Bickenbach

Key Words: AISI 416; UNS S41600; ASTM A314; A473; A484; A581; A582; F899; AMS 5610; QQ-S-763; QQ-S-764; MIL-W-52263; SAE J405 51416; EN 10088-3 1.4401/1.4005, X12CrS13
Vendors:
Available Properties
  • Density
  • Hardness, Brinell, Heat Treatment (Condition T HRc 26-32)
  • Hardness, Brinell, Turned Bars
  • Hardness, Brinell, Cold Drawn Bars
  • Tensile Strength, Heat Treatment (Condition T HRc 26-32)
  • Tensile Strength, Turned Bars
  • Tensile Strength, Cold Drawn Bars
  • Tensile Strength, Yield, Heat Treatment (Condition T HRc 26-32)
  • Tensile Strength, Yield, Turned Bars
  • Tensile Strength, Yield, Cold Drawn Bars
  • Elongation at Yield, Heat Treatment (Condition T HRc 26-32)
  • Elongation at Yield, Cold Drawn Bars
  • Elongation at Yield, Turned Bars
  • Reduction of Area, Heat Treatment (Condition T HRc 26-32)
  • Reduction of Area, Cold Drawn Bars
  • Reduction of Area, Turned Bars
  • Tensile Modulus
  • Electrical Resistivity
  • CTE, linear
  • Thermal Conductivity
  • Annealing Temperature, Sub-critical anneal
  • Annealing Temperature, Softest Properties
  • Annealing Temperature, Hold for time, slow cool
  • Hot-Working Temperature, Slow heating
  • Hot-Working Temperature, Forging range
  • Hot-Working Temperature, Then more rapidly
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Phosphorus, P
  • Silicon, Si
  • Sulfur, S
  • Zirconium, Zr
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Schmolz + Bickenbach (Swiss Steel International)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.