MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Go Yen Chemical GY-FROP31 Non-Halogenated Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GY-FR-OP31 is synthetic flame retardant, mainly applied on coating and all kinds of resin application. It is a non halogen based with excellent stability properties. GY-FR-OP31 provides long term flame retard ability for end product with good compatibility with different kinds of fabric.

Intro: GY-FR OP31 is synthetic flame retardant, mainly applied on coating and all kinds of resin application. It is a non halogen based with excellent stability properties. GY-FR-OP31 provides long term flame retard ability for end product with good compatibility with different kinds of fabric.

Advantages:

  • Confer end product long term flame retard ability
  • Belong to non halogen (no fluorine, chlorine, bromine, halogen element) flame retardant
  • Compounding with GY-FR-OP31 can reduce black smoke generated
  • Provide good decomposition temperature
  • Low specific gravity and corrosion/ low density smoke
  • Won’t produce migration while adding GY-FR-OP31
  • Good compatible with all kinds of paint, plastic, polymer, resin, elastomer, foam, adhesive compounding
Applications:
  • Paint, Coating and various resin: Flame retard paint & coating, powder coating, acrylic product required flame retardant, polyurethane resin, PMMA, latex resin, adhesive related product
  • Thermoplastic plastic : PP, PE, HDPE, LDPE, PC, POLYOLIFIN,POLYESTER RESIN , NYLON, POM, PBT, engineering plastic…etc
  • Textile application
  • Rubber and Elastomer industry: All kinds of nature and synthetic rubber : TPE, SBS, SEBS
  • Various of foam and flame retard foaming products
  • Polyamide like (polyamide 66, 6, 11, 12)
  • Various of foam and flame retard foaming products
  • Polyurethanes Type(TPU, PU RESIN ) Electronic products made from TPU: Switch, connector, covering

Information provided by Go Yen Chemical

Vendors:
Available Properties
  • Density
  • Particle Mesh Size
  • pH
  • Decomposition Temperature
  • Moisture Content
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.