TAIPOL® 6150 is a linear triblock copolymer with 29% styrene content. The product exhibits the following characteristics: - Medium to Low molecular weight
- Superior weather and heat resistance
- Good compatibility with plastics and oils
- Suitable for footwear, adhesives, sealants, coatings, asphalt modification, plastic modification and thermoplastic elastomer compound
Information provided by TSRC Corporation |