Available Properties |
---|
- Volatiles
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 03, 14 days at 160°F (71°C), 100% R.H.
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 03, 14 days at 160°F (71°C), 100% R.H.
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 05, 14 days at 160°F (71°C), 100% R.H.
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 03
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 03
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 05, 14 days at 160°F (71°C), 100% R.H.
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 05
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 03
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 03
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 03
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 03
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 05
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 05
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 05
- Tensile Strength, Honeycomb Flatwise, Note 1, Grade 05
- Tensile Strength, Honeycomb Flatwise, Note 2, Grade 05
- Shear Strength, Sandwich Beam, Note 2, Grade 03
- Shear Strength, Sandwich Beam, Note 1, Grade 03
- Shear Strength, Sandwich Beam, Note 1, Grade 05
- Shear Strength, Sandwich Beam, Note 2, Grade 05
- Shear Strength, Sandwich Beam, Note 1, Grade 03
- Shear Strength, Sandwich Beam, Note 1, Grade 05
- Shear Strength, Sandwich Beam, Note 2, Grade 05
- Shear Strength, Sandwich Beam, Note 2, Grade 03
- Shear Strength, Sandwich Beam, Note 1, Grade 03
- Shear Strength, Sandwich Beam, Note 1, Grade 05
- Shear Strength, Sandwich Beam, Note 2, Grade 03
- Shear Strength, Sandwich Beam, Note 2, Grade 05
- Shear Strength, Double Lap, Note 1, Grade 05
- Shear Strength, Double Lap, Note 1, Grade 03
- Shear Strength, Double Lap, Note 2, Grade 03
- Shear Strength, Double Lap, Note 2, Grade 05
- Shear Strength, Double Lap, Note 2, Grade 05, 14 days at 160°F (71°C), 100% R.H.
- Shear Strength, Double Lap, Note 1, Grade 05, 14 days at 160°F (71°C), 100% R.H.
- Shear Strength, Double Lap, Note 2, Grade 03, 14 days at 160°F (71°C), 100% R.H.
- Shear Strength, Double Lap, Note 1, Grade 05
- Shear Strength, Double Lap, Note 2, Grade 05
- Shear Strength, Double Lap, Note 1, Grade 03
- Shear Strength, Double Lap, Note 1, Grade 03, 14 days at 160°F (71°C), 100% R.H.
- Shear Strength, Double Lap, Note 2, Grade 03
- Shear Strength, Double Lap, Note 2, Grade 03
- Shear Strength, Double Lap, Note 1, Grade 05
- Shear Strength, Double Lap, Note 2, Grade 05
- Shear Strength, Double Lap, Note 1, Grade 08, 14 days at 160°F (71°C), 100% R.H.
- Shear Strength, Double Lap, Note 2, Grade 08, 14 days at 160°F (71°C), 100% R.H.
- Shear Strength, Double Lap, Note 1, Grade 03
- Shear Strength, Double Lap, Note 1, Grade 03
- Shear Strength, Double Lap, Note 2, Grade 05
- Shear Strength, Double Lap, Note 1, Grade 08
- Shear Strength, Double Lap, Note 1, Grade 05
- Shear Strength, Double Lap, Note 2, Grade 03
- Shear Strength, Double Lap, Note 2, Grade 08
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Glass Transition Temp, Tg
|
| | |