MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Materion Aluminum Oxide Al2O3 for Optical Coating
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Aluminum oxide, Al2O3, is a medium index, low absorption material usable for coatings in the near-UV (<300 nm) to IR (9 µm) regions. Typical applications include near-UV laser AR and dielectric mirror designs. Alumina can be used in combination with silicon dioxide layers to form multi-layer structures with high damage thresholds for UV laser applications. Completely oxidized alumina films are absorption-free over the range below 300 nm to at least 5 µm. Slight dissociation and oxygen loss occurs during evaporation. Adhesion is good to glass, most other oxides, some polymers, and to metals such as aluminum and silver. The films generally grow with a crystalline microstructure and low packing density and exhibit index changes when vented to moist air. Adsorption of water is often evident as rings of discoloration which reach a uniform appearance after moisture penetration is complete. This instability effect is exaggerated under low energy evaporation, low substrate temperature, or excessive background pressure evaporation conditions. The refractive index responds to high energy deposition techniques and to high substrate temperature because both parameters decrease the void volume by increasing the packing density of the microstructure. Post-deposition baking in air can also raise the refractive index.

Information provided by Materion.

Vendors:
Available Properties
  • Density, Crystal
  • Molecular Weight
  • Melting Point
  • Refractive Index
  • Refractive Index
  • Refractive Index
  • Refractive Index
  • Refractive Index
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Materion Corporation (former Williams Advanced Alloys)

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.