MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Omnia Plastica PEEK Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: Semicrystalline polymer. Material with high mechanical and thermal properties, up to 240°C. It resists to creep under load and to wear, its friction coefficient is low. The temperature resistance without load is high but it is reduced by the addition of load even if limited.

Features:

  • High temperature. It resists beyond 240°C. (The Heat distortion temperature is 162°C)
  • Dimensional stability
  • Good chemical resistance
  • Good abrasion resistance and low friction coefficient.
  • Electrically insulation
Weak Point:
  • Very high cost.
  • Load bearing decreases above 140° C.
  • Not inherently U.V. stable.
Application:
  • Mechanical: The dimensional stability at temperature is high, as well as the heat resistance. The components obtained have a high wear resistance and are self-lubricated. It is used to high performance pieces at low as well as at high temperatures:gears bushes, in aircraft and aerospace industries.
  • Electrical: Very good dielectric and insulating properties.
  • Chemical: Very good chemical resistance. Ball valve seals, pump housings
  • Nuclear: High resistance to gamma radiation

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors:
Available Properties
  • Density, ISO.1183 DIN.53479
  • Moisture Absorption at Equilibrium, 50% relative humidity
  • Water Absorption at Saturation, 23°C
  • Hardness, Rockwell M, ISO2039.2, dry sample
  • Tensile Strength at Break, ISO.527 DIN.53455
  • Elongation at Break, ISO.527 DIN.53455
  • Tensile Modulus, ISO.527 DIN.53455
  • Charpy Impact Unnotched, ISO.R179 DIN.53453, 7.5 J
  • Charpy Impact, Notched, ISO179/3C DIN.53453
  • Volume Resistivity, ISO.93 DIN.53482
  • Dielectric Constant, ISO.250 DIN.53483
  • Dielectric Strength, ISO.243 DIN.53481
  • Dissipation Factor, ISO.250 DIN.53483
  • CTE, linear
  • Thermal Conductivity, DIN.52612
  • Melting Point
  • Maximum Service Temperature, Air, Continuous; 5000 hours based on a tensile stress of 50% at 23° C.
  • Maximum Service Temperature, Air, short period, no load
  • Deflection Temperature at 1.8 MPa (264 psi), ISO.75 DIN.53461
  • Minimum Service Temperature, Air, impact conditions and heavy loads not considered
  • Flammability, UL94
  • Oxygen Index, ISO.4589
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Omnia Plastica s.p.a.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.