MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Carlson C 825 Nickel-Iron-Chromium Alloy
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy

Material Notes: General Description

Carlson Alloy C 825 is a nickel-iron-chromium alloy, developed for use in extremely corrosive environments. The nickel content of this alloy makes it resistant to chloride-ion stress corrosion cracking; and in combination with its molybdenum and copper content, endows C 825 with resistance to oxidizing environments. When heated in the critical sensitization temperature range of 1200°F to 1400° (650°C to 760°C), C 825 resists pitting and intergranular attack.

Applications

C 825 is utilized in numerous corrosive environments, including the processing and storage of reducing acids such as sulfuric and phosphoric solution. It is also used in various oxidizing environments, including nitric and acid solutions, nitrates and oxidizing salts.

C 825 offers excellent resistance to corrosion by sea water

  • Chemical Processing – heat exchangers, evaporators, pumps, piping, valves, vessels, expansion bellows, tank trucks, scrubbers, condensers, tank and vessel linings; and for processing and handling sulfuric acid, phosphoric acids, hydrofluoric acid, nitric acid, nitrates and oxidizing salts.
  • Pulp and Paper – wet scrubber linings in systems using sodium sulfite and sodium bisulfate solutions.
  • Pickling Processes – tank heaters and hooks
  • Ore Processing – hydrometallurgy and plate heat exchangers in copper refining.
  • Pollution Control – Hopper bottoms and trays in electrostatic precipitators; ducts and dampers, stack-gas reheaters, waste heat recovery exchangers, stack liners and other wet scrubber components; sludge-incinerator wet scrubbers; marine inert-gas scrubbers; radwaste evaporator systems.

Information provided by Carlson

Key Words: UNS N08825
Vendors:
Available Properties
  • Density
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Modulus of Elasticity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Electrical Resistivity
  • Magnetic Permeability, 200 Oersted
  • Curie Temperature
  • CTE, linear
  • CTE, linear
  • CTE, linear
  • Melting Point
  • Solidus
  • Liquidus
  • Aluminum, Al
  • Carbon, C
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Manganese, Mn
  • Molybdenum, Mo
  • Nickel, Ni
  • Silicon, Si
  • Sulfur, S
  • Titanium, Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.