MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Wanshijie APET Sheet
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: APET sheet has excellent air-tightness, durability, chemical resistance and transparency. When burnt, it will not produce any toxic gas, so it is environment friendly. Also it complies with American FDA and Japanese food safety standard. It has become the safety material for foodstuff. In addition, it is applicable for various machining, displaying or exhibiting, vacuum forming and etc.

GOOD TRANSPARENCY: It has above 87 percent of transparency and good texture touch and is suitable for the products that require high transparency.
EXCELLENT IMPACT STRENGTH RESISTANCE AND RIGIDITY: Hard and durable material, good physical property even at 40°C,suitable for the products that require high Impact strength resistance.
EXCELLENT THERMOFORMING: Be able to form when preheating is not needed, high precision, about 0.5 percent shrinkage, excellent deep thermoforming, even thickness and no crack.
EXCELLENT FOOD SAFETY: APET material can comply with all main food regulations, such as FDA or BGA. Suitable for food container packing.
EXCELLENT GREASE AND CHEMICAL RESISTANCE: No corrosion to acid, alkali, oil and etc.
LOW COMBUSTIBILITY: Excellent fire resistance, no support combustion, less smoke, no harmful substances after combustion.
ENVIRONMENT PROTECTION: Available to recycle and no environment pollution.

Vendors:
Available Properties
  • Specific Gravity, ASTM D1050
  • Film Tensile Strength at Yield, MD, ASTM D638
  • Film Tensile Strength at Yield, TD, ASTM D638
  • Elongation at Yield, ASTM D638
  • Modulus of Elasticity, ASTM D638
  • Flexural Modulus, ASTM D790
  • Heat Distortion Temperature, ASTM D648
  • Transmission, Visible, ASTM D1003
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Wanshijie Plastic Sheet Co

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.