MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Saint-Gobain Norton® ETFE Fluoropolymer Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: Features/Benefits:
  • Superior release properties
  • Excellent weatherability
  • Performance from -200°C (-328°F) to 165°C (330°F)
  • Excellent chemical and mechanical properties
  • Thermoformable
  • Product thicknesses from 0.0005" (0.0127 mm) to 0.020 (0.5 mm)
  • Width up to 62" (1575 mm) for 0.0005" to 0.010" and up to 48" for 0.010" - 0.020"
  • Blue, red and custom colors available
  • Available in cementable (surface treated) form

High Yield Fluoropolymer Film
Norton® ETFE fluoropolymer film is manufactured from a copolymer of ethylene and tetrafluoroethylene resin. This material offers the outstanding performance of fluoropolymer film over a temperature range from cryogenic to 165°C (330°F). The resistance to chemicals and weathering, low flammability, and stress crack resistance make this film an excellent candidate for a wide variety of applications.

Weatherable Applications
Norton® ETFE film offers excellent mechanical properties and tear resistance. The high light transmission (>95%) of Norton® ETFE film, when combined with its excellent mechanical and chemical properties, provides excellent performance in architectural roofing designs and greenhouses. Norton® ETFE film is also an excellent choice in solar collector applications due to its outstanding physical properties and high coverage factor resulting from its low density.

Low Surface-energy Applications
Norton® ETFE film offers a low surface energy, making it an excellent choice for release applications up to 350°F process temperature. The low density of this material, compared to Norton® FEP film, provides greater coverage per pound for composite molding release film applications. The low surface energy of Norton® ETFE can also be utilized in applications such as wall coverings and anti-graffiti protection for high traffic areas.

Fabrication Capabilities
Norton® ETFE film offers processors excellent dimensional stability for secondary processing such as thermoforming and welding. Products utilizing Saint-Gobain's surface treatment technologies, such as C-treatment, improve bondability characteristics for metalizing processes and adhesive coating.

Surface Treatments Available: C-Treatable (cementable, 1 or 2 sides); Corona Treatment (1 or 2 sides); Chemical Etching (1 or 2 sides)
Flammability (UL-94) = V-0
Used for Aerospace/Release Films, Chemical Process, Electrical/Electronics, Medical, Protective/Decorative.

Specification Notes: All values represent typical performance properties and should not be used for specification purposes.
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D-792
  • Water Absorption
  • Tensile Strength, Yield, ASTM D-882
  • Elongation at Break, ASTM D-882
  • Tensile Modulus, ASTM D-882
  • Elmendorf Tear Strength, MD, ASTM D-1922, (direction not reported), Propagation Tear Strength
  • Surface Resistivity per Square, ASTM D-257
  • Dielectric Constant, ASTM D-150
  • Dielectric Strength, ASTM D-149
  • Dissipation Factor, ASTM D-150
  • CTE, linear, ASTM D-696
  • Specific Heat Capacity
  • Thermal Conductivity, ASTM D-2863
  • Melting Point, ASTM D-3418
  • Maximum Service Temperature, Air, UL-746 B
  • Flammability, UL94
  • Oxygen Index, ASTM D2863
  • Refractive Index, ASTM D542
  • Transmission, Visible, ASTM E424
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.