MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
LG Chemical LUTENE® XL2700BK TR Crosslinkable Semiconductive Shielding Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Applications: Cross-linkable, easy strippable semi-conductive insulation shielding compound for medium voltage power cables with rated voltage up to 35kV

Description: L

  • UTENE® XL2700BK TR was specially designed cross-linkable semi-conductive compound for easy strippable insulation shielding of medium and high voltage power cable.
  • LUTENE® XL2700BK TR provides an excellent stripping property, lower and consistent stripping force over a wide temperature range without tearing, leaving a clean insulation surface.
  • LUTENE® XL2700BK TR is recommended for use in conjunction with XL8080NTS (Cross-linked polyethylene compound) and XL8080TR (Tree-retardant cross-linked polyethylene compound).
Characteristics:
? Excellent Surface Smoothness
? Excellent Electrical Properties
? Outstanding Strippability

Specification: LUTENE® XL2700BK TR meets the property requirement of the following material specifications.
? AEIC CS8
? ICEA S-94-649, S-93-639 / NEMA WC74
? IEC 60502
? CENELEC HD620
? BS 6622

Information provided by LG Chemical

Vendors:
Available Properties
  • Density, ASTM D1505, Base Resin
  • Tensile Strength at Break, ASTM D638, 200 mm/min
  • Tensile Strength at Break, ASTM D638, retention after
  • Elongation at Break, ASTM D638, 200 mm/min
  • Elongation at Break, ASTM D638, retention after
  • Volume Resistivity, ASTM D991, DC
  • Volume Resistivity, ASTM D991, DC
  • Brittleness Temperature, ASTM D746, no crack
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.