MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
AGC LUMIFLON® LF-9716 Fluoropolymer Resin
Categories: Polymer; Thermoset; Fluoropolymer, TS

Material Notes: LUMIFLON fluoropolymers consist of alternating fluoroethylene and vinyl ether segments (FEVE). The fluorinated segments provide outstanding UV resistance and weatherability as well as chemical resistance, while the vinyl ether segments provide crosslinking sites. LUMIFLON LF-9716 and LF-9721 have extremely high hydroxyl functionality and have a high crosslink density after reaction with isocyanates. These resins are useful wherever excellent chemical resistance is required. Typical applications include coatings for aerospace, tank lining, water tanks, and military coatings.

Product Characteristics:

  • Excellent chemical resistance
  • High erosion resistance
  • Offered in EEP HAPS free solvent
  • High solids

Information provided by AGC Chemicals Americas Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Viscosity
  • Gardner Color Number
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.