MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Mitsubishi Chemical Advanced Materials RCH® 1000 Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: RCH 1000 Ultra High Molecular Weight UHMW-PE is a highly versatile, ultra-high molecular weight plastic that is ideal for many orthotic applications. It has a forming temperature of +180°C, is suited for deep-drawing and has an excellent stability. RCH 1000 PE-UHMW is used for ankle foot orthoses, body jackets, upper limb orthoses and especially for orthopedic insoles.

Vendors:
Available Properties
  • Density, ISO 1183-1
  • Water Absorption, ISO 62, Immersion
  • Water Absorption at Saturation
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Ultimate, ISO 527-1/-2
  • Elongation at Break, ISO 527-1/-2
  • Modulus of Elasticity, ISO 527-1/-2
  • Charpy Impact Unnotched, ISO 179-1/1eU
  • Charpy Impact, Notched, ISO 21304-2, double 14° notched
  • Sand Slurry, ISO 15527, based on TIVAR®1000 = 100
  • Surface Resistivity per Square, ANSI/ESD STM 11.11
  • CTE, linear
  • Melting Point, ISO 11357-1/-3, DSC, 10°C / min
  • Maximum Service Temperature, Air, Continuous (20.000 hrs)
  • Minimum Service Temperature, Air
  • Flammability, UL94
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Mitsubishi Chemical Advanced Materials (former Quadrant Engineering Plastics Products)

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.