Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America
Features: Abrasion Resistant; Good Flexibility; Halogen Free; Heat Aging Resistant; High Elongation; High Hardness; High Tensile Strength; Low Temperature Flexibility; Medium Density; Medium Flow; Sunlight Resistant; UV Resistant; Weather Resistant
Uses: Appliance Wire Insulation; Appliance Wire Jacketing. Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Rubber Replacement; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing
RoHS Compliance: RoHS Compliant
Form: Pellets
Processing Method: Injection Molding; Extrusion
This page displays only the textof a material data sheet.To see MatWeb's complete datasheet for this material (includingmaterial property data, metalcompositions, material suppliers,etc), please click the button below.
Category NotesPlasticThermoplastic Elastomer