MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
NOVA Chemicals Sclair® 2114 LLDPE Injection Molding Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes:

Butene Copolymer

Features:

  • Excellent processability, cold temperature impact resistance and ESCR properties
  • Outstanding flexibility and warpage resistance
  • Good organoleptic properties and natural color
  • High surface gloss

Additives:

  • Processing antioxidant

Applications:

  • Thin wall lids for frozen food packaging (ice cream, whipped dairy)
  • Caps and closures, tamper evident, dairy applications
  • Compounding

United States: SCLAIR 2114 resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 3.1a, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.

Data provided by the manufacturer.

Key Words: Linear Low Density Polyethylene
Vendors:
Available Properties
  • Density, ASTM D792
  • ESCR 100% Igepal®, F50, Condition A, ASTM D1693
  • Melt Flow, ASTM D1238
  • Spiral Flow, NOVA Snake Flow Test
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Yield, ASTM D638, 50 mm/min
  • Tensile Strength, Yield, ASTM D638, 500 mm/min
  • Elongation at Break, ASTM D638, 500 mm/min
  • Elongation at Break, ASTM D638, 50 mm/min
  • Flexural Modulus, ASTM D790
  • Vicat Softening Point, ASTM D1525
  • Brittleness Temperature, ASTM D696
  • Melt Temperature
  • FDA, See notes for details.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.