MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Kohesi Bond KB 10473 FLV Two component, low viscosity, flexible epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • Superior optical clarity
  • Excellent flow properties
  • Phenomenal flexibility
  • Very low exotherm, ideal for casting
  • Exceptional electrical insulation properties
  • Resists mechanical and thermal shocks
Kohesi Bond KB 10473 FLV is a two component, room temperature curing epoxy system suitable for bonding, sealing, potting and encapsulation. It has a convenient 1:1 (Part A: Part B) mix ratio by weight. This epoxy system offers excellent flexibility and peel strength. It readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 10473 FLV is optically clear and offers top notch light transmissions properties. It has a refractive index of 1.51. It offers an extensive service temperature range of 4K (-269.15°C) to +120°C. This adhesive fosters outstanding resistance to mechanical and thermal shocks, even at cryogenic temperatures. It offers minimal shrinkage upon cure. KB 10473 FLV adheres well to a wide variety of substrates including metals, ceramics, most plastics and glass. In addition to superior electrical insulation, it also offers lower exotherm, making it ideal for stress free bonding. Part A and Part B are clear in color. KB 10473 FLV is widely used in optical, optoelectronic, fiber-optic, electronics and related industries especially where optical clarity, cryogenic serviceability and high flexibility are desired.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Viscosity, Part A
  • Viscosity, Part B
  • Hardness, Shore D
  • Tensile Strength
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Peel Strength, Al/Al
  • Volume Resistivity
  • Dielectric Constant
  • CTE, linear
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Refractive Index
  • Cure Time, Option 2
  • Cure Time, Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
  • Cure Time, Option 1
  • Working Life, 100 g of mixed epoxy
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.