MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Kohesi Bond TUF 1621 AOHT Toughened, two component epoxy for bonding and sealing
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Product Highlights:
  • Superior thermal conductivity
  • Excellent toughness
  • Convenient 1:1 mix ratio
  • First-rate thermal conductivity
  • Exceptional electrical insulation properties
  • Capable of passing NASA low outgassing
Kohesi Bond TUF 1621 AOHT is a two component, room temperature curing epoxy system suitable for bonding and sealing. It is capable of passing NASA standards for low outgassing (ASTM E-595) and has a convenient 1:1 (Part A: Part B) mix ratio by weight or volume. This epoxy system offers excellent toughness and superior peel strength. It readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. TUF 1621 AOHT is thermally conductive and it can withstand very high temperatures. It offers an extensive service temperature range of -70°C to +204°C. This adhesive fosters outstanding resistance to mechanical and thermal shocks. It offers exceptionally high lap shear strength. TUF 1621 AOHT adheres well to a wide variety of substrates including metals, ceramics, most plastics, rubbers and glass. In addition to superior electrical insulation, it also offers very good resistance to various chemicals, such as water, oils and fuels. Part A and Part B are gray/off-white in color. TUF 1621 AOHT is widely used in electronic, optoelectronic, vacuum, aerospace and related industries.

Typical Applications:

  • Coating
  • Bonding
  • Sealing

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors:
Available Properties
  • Viscosity, Part A
  • Hardness, Shore D
  • Tensile Modulus
  • Adhesive Bond Strength, Tensile Lap Shear, Al/Al
  • Peel Strength, Al/Al
  • Volume Resistivity
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time, Option 2
  • Cure Time, Optimum Cure: overnight at 23°C plus 3 - 5 hours at 70°C - 90°C
  • Cure Time, Option 1
  • Working Life, 100 g of mixed epoxy
  • Shelf Life, in original unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.