MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Aluminum Bronze, UNS C61300, H04 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked, Capacity for Being Hot Formed; Fair Suitability – Brazing

Common Fabrication Processes: Blanking; Cold Heading; Drawing; Forming and Bending; Roll Threading; Welding

Typical uses: Wire Screening; Bolts; Fasteners; Nuts; Columns; Condenser Tube; Corrosion Resistant Vessels; Desalination Equipment; Gaskets; Heat Exchanger Tube; Machine Parts; Mining Shovels; Piping Systems, Acid Resistant; Sea Water Piping; Seamless Tubing and Pipe; Tanks; Tie Rods; Tube Sheets; Water Boxes; Protective Sheathing; Blending Chambers; Mixing Troughs; Ball Valve Seats

Applicable Specifications: Bar – FEDERAL QQ-C-450, ASTM B150/B150M, ASTM B169/B169M; Pipe – ASTM B608; Plate – FEDERAL QQ-C-450, ASTM B432, ASTM B169/B169M; Plate & Sheet - for Pressure Vessels, Condensers & Heat Exchangers ASTM B171/B171M, for Pressure Vessels, Condensers & Heat Exchangers ASME SB171; Rod – ASTM B150/B150M; Rod, Bar & Shapes - Aluminum Bronze ASME SB150; Rod, Tubing & Shapes - Aluminum Bronze ASTM B150/B150M; Seamless Condenser Tube & Ferrule Stock – ASME SB111, ASTM B100; Seamless Pipe and Tube – ASTM B315, ASME SB315; Sheet – FEDERAL QQ-C-450, ASTM B169/B169M; Sheet, Strip & Rolled Bar - Aluminum Bronze ASME SB169; Strip – FEDERAL QQ-C-450, ASTM B169/B169M; Tube – ASTM B111/B111M

Vendors:
Available Properties
  • Density
  • Hardness, Rockwell B
  • Hardness, Rockwell B
  • Hardness, Rockwell B
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength
  • Tensile Strength, Yield, 0.5% Ext
  • Tensile Strength, Yield, 0.5% Ext
  • Tensile Strength, Yield, 0.5% Ext
  • Elongation at Break
  • Elongation at Break
  • Elongation at Break
  • Tensile Modulus
  • Modulus of Rigidity
  • Poissons Ratio, Calculated
  • Fatigue Strength
  • Machinability
  • Forgeability
  • Shear Strength
  • Shear Strength
  • Shear Strength
  • Electrical Resistivity, 12% IACS
  • CTE, linear
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Annealing Point
  • Hot-Working Temperature
  • Aluminum, Al
  • Copper, Cu, As Balance
  • Iron, Fe
  • Lead, Pb
  • Manganese, Mn
  • Nickel, Ni
  • Phosphorus, P
  • Silicon, Si
  • Tin, Sn
  • Zinc, Zn
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.