Cobalt neodecanoate 6% solution for curing unsaturated polyester resins. Cobalt neodecanoate has milder CRM classification and is therefore preferred over Cobalt octoate. Applications: The curing of unsaturated polyester resins at ambient temperatures can in general not be performed by an organic peroxide alone. The radical formation, which is necessary to start the polymerization reaction, is at ambient temperatures with most generally applied organic peroxides too slow. To speed up the radical formation in a controllable way organic peroxides must therefore be used in combination with a so called accelerator. CAS number 27253-31-2 EINECS/ELINCS No.: 248-373-0 Information provided by Nouryon |