MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
GEHR Plastics POM-10PE Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear because of the high strength and smooth surface. There is a very low risk of stress cracks. POM-C exhibits a high thermal stability and a high resistance to chemicals. Improved sliding properties for applications with increased abrasion.

Properties:

  • no microporosity
  • high strength
  • high rigidity
  • high thermal stability
  • low water absorption
  • high dimension stability
  • good electrical insulating properties
  • very good sliding properties
  • high resistance to stress cracks
  • not resistant to high concentrated acids
  • difficult to glue and paint
Applications include bearings, fittings, gear wheels, parts for pumps, screws, bobbins, parts for textile industry, and medium for coating lines.

Vendors:
Available Properties
  • Specific Gravity, ISO 1183
  • Moisture Absorption at Equilibrium, ISO 62
  • Water Absorption at Saturation, ISO 62
  • Hardness, Shore D, ISO 868
  • Tensile Strength, Yield, ISO 527
  • Elongation at Break, ISO 527
  • Elongation at Yield, ISO 527
  • Modulus of Elasticity, ISO 527
  • Charpy Impact Unnotched, ISO 179
  • Charpy Impact, Notched, ISO 179
  • Volume Resistivity, IEC 60093
  • Surface Resistance, IEC 60093
  • Dielectric Constant, IEC 60250
  • Dielectric Strength, IEC 60243-1
  • Dielectric Loss Index, IEC 60250
  • Comparative Tracking Index, IEC 60112
  • CTE, linear, ISO 11359
  • Thermal Conductivity, ISO 22007-4
  • Melting Point, DIN EN ISO 3146
  • Maximum Service Temperature, Air, UL 746B
  • Deflection Temperature at 1.8 MPa (264 psi), ISO 75
  • Minimum Service Temperature, Air, UL 746B
  • Glass Transition Temp, Tg, DIN EN ISO 3146
  • Flammability, UL94, UL 94
  • FDA, Physiological indifference
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
GEHR Plastics Inc

Category Notes
Plastic
POM, Polyoxymethylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.