MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
ChevronTexaco RPM® SAE 50 Synthetic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Features

Chevron RPM Synthetic Transmission Fluid is a heavy duty truck manual transmission fluid.

It is manufactured from synthesized hydrocarbon base fluids which have excellent thermal and oxidation stability, a high natural viscosity index, and a very low pour point.

This product possesses excellent shear stability even under heavily loaded conditions.

The low pour point and low temperature fluidity of Chevrons RPM Synthetic Transmissions Fluid imparts improved lubrication during startup at subzero temperatures, while the improved viscosity-temperature characteristics provide dependable lubrication at high temperatures. Lower frictional losses in the lubricant film and reduced churning losses, due to lower bulk oil viscosity, reduce operating temperatures significantly when compared to conventional mineral based lubricants.

Applications

Chevron RPM Synthetic Transmission Fluid’s outstanding low temperature flow properties and natural high viscosity index provides superior all-climate, year-round performance in heavy duty truck transmissions.

Its use permits easier shifting in extremely cold weather and less drag and gear wear during startup.

This product is not recommended for use as an engine crankcase oil.

Key Words: CPS Number: 210456; MSDS Number: 4896
Vendors:
Available Properties
  • API Gravity
  • Brookfield Viscosity
  • Brookfield Viscosity
  • Brookfield Viscosity
  • Brookfield Viscosity
  • Brookfield Viscosity
  • Brookfield Viscosity
  • Viscosity Measurement, ASTM D2270, Viscosity Index
  • Saybolt Viscosity at 100°F
  • Saybolt Viscosity at 210°F
  • Kinematic Viscosity at 40°C (104°F), ASTM D445
  • Kinematic Viscosity at 100°C (212°F), ASTM D445
  • Pour Point, ASTM D97
  • Flash Point, ASTM D92
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
ChevronTexaco Corp

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

New MatWeb Services
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.