MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Saint-Gobain COHRlastic® F-12 Silicone Foam
Categories: Polymer; Thermoset; Silicone; Silicone Foam

Material Notes: Description: Low-density, flame-retardant COHRlastic silicone foam yard goods provide outstanding performance for industries ranging from aviation and mass transit to automotive, electronics, construction and furniture. In addition to a UL94V-O listing in thicknesses down to 1/16", it withstands a 2100°F flame for more than 10 minutes without burning through in thicknesses down to 3/8". The material, which has a nominal density of 12 pounds per cubic foot, generates very little white smoke. Non-corrosive for use with metals and in hostile environments, it has low compression set. Among its applications are fireblocks, thermal barriers, noie and vibration dampeners, insulationa dn high-performance gaskets or seals. For the aviation, automotive and mass transit industries, it offers a high degree of design flexibility. Lightweight and easy to process, it can be laminated to seat cover fabrics and carpeting as a backing for added flame resistance in passenger compartment furnishings. The material has similar uses in institutional and residential furnishings, marine and lighting applications. It offers properties valuable in flame retardant backings for floor, wall and furniture coverings; fire-wall and thermal barriers or insulation, padding and gasketing for commercial and private marine vehicles; or gasketing and sealing in high-intensity light fixtures and electronic components in medial, computer and business equipment. Supplied in 18" and 36" wide roll stock. Thicknesses are shown in the table below. It is available plain or, on special order, laminated to any of a wide range of substrates. Because of the unique nature of COHRlastic foam, SGPPL CHR has undertaken a rigorous testing program which is performed at outside independent laboratories. The tests document the flame resistant properties and low levels of toxicity and smoke generation as well as mechanical and electrical properties. Details are on file at SGPPL CHR.
  • Passes FDA Extractables, 21 CFR177.2600
  • Products Combustion (ASTM E662), Hydrogen Cyanide = 0 ppm
  • In compliance with Boston Fire Dept. Chair Test, January 1986
  • Passes FAR 25.853(a) and (b)
  • Passes UL94V-0
All data based on a 0.0625 inch test sample.(Other thicknesses available.)
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Density
  • Tensile Strength, Yield
  • Elongation at Break
  • Compressive Strength, ASTM D1056, Compression Deflection, Compressed to 75% original thickness.
  • Compression Set, Constant Deflection, Compressed 50% for 22 hrs
  • Insulation Resistance, ASTM D257
  • Insulation Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Arc Resistance, ASTM D495
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flammability, UL94
  • Flame Spread Index, ASTM E162
  • Flame Spread Index, ASTM D3675, Radiant Panel
  • Smoke Density, ASTM E662, 4 minutes, flaming mode
  • Smoke Density, ASTM E662, 4 minutes, smoldering mode
  • Oxygen Index, ASTM 2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.