MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Rubaloy Rubaloy 2530 NBR / PVC
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Product Information: Rubaloy – 2530 is a unique blend of Oil Extended Nitrile Rubber and Polyvinyl Chloride with a very high percentage of Plasticizers, etc. Test reports have proved that Rubaloy-2530 has excellent processing qualities. This grade has substantial tensile strength, especially considering the total percentage of plasticizer that has been infused into it. This grade is also resistant to solvents and mild acids, which makes it ideal for printing rollers. Handling, cutting and weighing of Rubaloy-SS is easy as it comes in soft sheets, thus saving on time, cost and labour.

Processing Characteristics: Rubaloy-2530 can be easily processed on conventional rubber mixing/compounding machines. It has excellent filler and plasticizer absorption properties and can withstand elevated compounding temperatures.

Curing: Sulphur or peroxide curing is recommended for Rubaloy - 2530. It has improved curing properties as compared to other similar polymers. A slightly higher dosage of accelerators is recommended.

Applications: Since Rubaloy-2530 has a relatively low polymer hardness, not found in NBR/PVC Blends it has a unique advantage to manufacture low hardness printing rollers, moulded articles, low density foam, soft pipes, tubes and hoses.

Information provided by Rubaloy™

Vendors:
Available Properties
  • Specific Gravity
  • Mooney Viscosity, ML 1+4
  • Hardness, Shore A
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.