MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800)
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: 100% expanded PTFE, with multi-directional strength. Resistant to all media in the 0-14 pH range, except molten alkali metals and element fluorine, particularly at elevated temperatures and pressures. Complies with FDA 21 CFR 177.1550 (PTFE) food requirements.

GORE Universal Pipe Gaskets are used to seal all types of flanges in chemical-process piping. Style 800 gaskets are designed to meet the needs of various piping materials. They are ideal for standardizing gasket material across steel, glass-lined steel, and FRP systems -- any application in which a non-metallic gasket can be used.

Key Features:

  • 100 percent expanded PTFE
  • Chemically inert and temperature resistant
  • Seals at low bolt load
  • Conforms to flange deviations
  • High dimensional stability
  • Resists creep and cold flow
  • Resistant to blowout
Key Benefits:
  • Seals all types of standard piping
  • Standardize: One gasket system-wide
  • Protects against use of wrong gasket
  • Lowers process emissions
  • Reliable sealing performance
  • Seldom needs retorquing
  • Lowers total sealing cost

Vendors:
Available Properties
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • FDA
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
W. L. Gore & Associates

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.