MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Melos Mecoline S TP 1005 F Halogen-free, thermoplastic, flame retardant sheathing
Categories: Polymer; Thermoplastic

Material Notes: Halogen-free, thermoplastic, flame retardant sheathing compound for low and medium voltage cables

Compound class: Sheathing

Compound category: TP

Flame retardant: ATH

Standards: VDE 0207 part 24 HM 2, HM 4; DIN EN 50363-8 TM7; BS 7655 section 6.1 LTS 1 - LTS 4; DIN VDE 0276-604 HM4; NF C 32-323; DIN VDE 0281 part 14 TM7; CEI 20-11 M1; VDE 0250 part 215 HM5; IEC 60092-360 SHF 1

Typical applications: Flame retardant halogen free and low smoke, oil resistant, ozone resistant, max. operating temperature 90°C.

Features: Flame retardant; Halogen-free; Low smoke; Oil resistant

Information provided by Melos

Vendors:
Available Properties
  • Density, DIN EN ISO 1183-1A, pressed plaques, 165°C / 5 min
  • pH, IEC 60754-2, Corrosivity, Acid gas emission
  • Mooney Viscosity
  • Melt Flow, DIN EN ISO 1133
  • Hardness, Shore D, DIN ISO 7619-1, pressed plaques, 165°C / 5 min
  • Tensile Strength, IEC 60811-501, extruded tapes
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 903
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 903
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, extruded tapes, Diesel Oil
  • Tensile Strength, IEC 60811-404, Petrol (super lead-free)
  • Tensile Strength, IEC 60811-404, Dot 4 acc. TL 6850-0017, Diesel Oil
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, Water
  • Tensile Strength, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Tensile Strength, IEC 60811-404, SAE 20
  • Tensile Strength, IEC 60811-401, extruded tapes, After ageing in air oven
  • Elongation at Break, IEC 60811-501, extruded tapes
  • Elongation at Break, IEC 60811-501, extruded tapes
  • Elongation at Break, IEC 60811-501, extruded tapes
  • Elongation at Break, IEC 60811-404, Dot 4 acc. TL 6850-0017, Diesel Oil
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 903
  • Elongation at Break, IEC 60811-404, extruded tapes, Diesel Oil
  • Elongation at Break, IEC 60811-404, Petrol (super lead-free)
  • Elongation at Break, IEC 60811-404, Water
  • Elongation at Break, IEC 60811-404, SAE 20
  • Elongation at Break, IEC 60811-401, extruded tapes, After ageing in air oven
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 903
  • Elongation at Break, IEC 60811-404, extruded tapes, Fluid IRM 902
  • Penetration, IEC 60811-508, [%] Hot pressure test, extruded tapes
  • Penetration, IEC 60811-508, [%] Hot pressure test, extruded tapes
  • Tear Strength, DIN 53 507, extruded tapes
  • Abrasion, DIN VDE 0472-605, [mm3], pressed plaques, 155°C / 5 min
  • Volume Resistivity, DIN VDE 0303-30, 10V
  • Volume Resistivity, DIN VDE 0303-30, 500V
  • Surface Resistance, DIN VDE 0303-31, 10V
  • Surface Resistance, DIN VDE 0303-31, 500V
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Brittleness Temperature, ASTM D 746-64T
  • Shrinkage, IEC 60811-509, extruded tapes
  • Processing Temperature, Tool
  • Processing Temperature, Maximum mass temperature
  • Zone 1
  • Zone 2
  • Zone 3
  • Zone 4
  • Zone 5
  • Adapter Temperature
  • Head Temperature
  • Drying Temperature
  • Dry Time
  • Shelf Life
  • Loss on Ignition(%), ASTM D 2863 A, pressed plaques, 165°C / 5 min.
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.