MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
BASF Palatinol® 11P-E (DUP) Linear Phthalate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Formula: C30H50O4

Description: Palatinol® 11P-E plasticizer is a linear phthalate ester based on a predominately linear C11 alcohol. Palatinol 11P-E exhibits very low volatility and good processing characteristics with vinyl resin. Its viscosity is relatively low in relation to its molecular weight. Palatinol 11P-E is inhibited with 0.1% by weight of 1,1,3-tris(2-methyl-4-hydroxy 5-t butylphenyl) butane.

Applications: Vinyl resin compounders choose Palatinol 11P-E over DTDP for its lower viscosity, greater resin compatibility, faster dry blending and superior efficiency. When formulated to equal concentrations, Palatinol 11P-E provides equal electrical properties in 90°C and 105°C wire insulation compounds. With its lower viscosity, high thermal resistance, permanence and low volatility, Palatinol 11P-E is well suited for demanding applications such as automotive interior (instrument panel skins), building wire insulation, 90° THW and 105° THW, automotive wire harness and vinyl roofing membrane.

Information provided by BASF

Vendors:
Available Properties
  • Density, ASTM D4052
  • Solubility of Water
  • Solubility in Water
  • Viscosity, Absolute
  • Viscosity, Absolute
  • Viscosity, Absolute
  • Molecular Weight
  • Vapor Pressure
  • Total Acid Number, ASTM D1045, [mg KOH/g]
  • Hardness, Shore A, ASTM D 2240, Plasticizer conc. in vinyl film 70 phr
  • Hardness, Shore A, ASTM D 2240, Plasticizer conc. in vinyl film 50 phr
  • Hardness, Shore A, ASTM D 2240, Plasticizer conc. in vinyl film 40 phr
  • Tensile Strength, ASTM D638, Plasticizer conc. in vinyl film 70 phr
  • Tensile Strength, ASTM D638, Plasticizer conc. in vinyl film 50 phr
  • Tensile Strength, ASTM D638, Plasticizer conc. in vinyl film 40 phr
  • Elongation at Break, ASTM D638, Plasticizer conc. in vinyl film 40 phr
  • Elongation at Break, ASTM D638, Plasticizer conc. in vinyl film 50 phr
  • Elongation at Break, ASTM D638, Plasticizer conc. in vinyl film 70 phr
  • 100% Modulus, ASTM D638, Plasticizer conc. in vinyl film 70 phr
  • 100% Modulus, ASTM D638, Plasticizer conc. in vinyl film 50 phr
  • 100% Modulus, ASTM D638, Plasticizer conc. in vinyl film 40 phr
  • Torsional Stiffness, ASTM D1043, Plasticizer conc. in vinyl film 40 phr
  • Torsional Stiffness, ASTM D1043, Plasticizer conc. in vinyl film 50 phr
  • Torsional Stiffness, ASTM D1043, Plasticizer conc. in vinyl film 70 phr
  • CTE, linear
  • Boiling Point
  • Pour Point
  • Brittleness Temperature, ASTM D746, Plasticizer conc. in vinyl film 70 phr
  • Brittleness Temperature, ASTM D746, Plasticizer conc. in vinyl film 50 phr
  • Brittleness Temperature, ASTM D746, Plasticizer conc. in vinyl film 40 phr
  • Flash Point
  • Refractive Index
  • Moisture Content, ASTM E203
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.