MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Chesterton ARC 855 Abrasion Control Coating
Categories: Ceramic; Polymer; Thermoset; Epoxy

Material Notes: An advanced ceramic composite formulated to protect equipment from aggressive chemical attack, corrosion, and erosion. The product is a low viscosity composite that is easily applied by brush or roller. ARC 855 may be applied at a minimum thickness of 250 microns (10 mills) per coat. Non-shrinking. 100% Solids. ARC 855 may be used alone, or in conjunction with other ARC composites. This two-coat system provides extended wear and predictable preventative maintenance. The cured ceramic composite provides outstanding chemical and abrasion resistance with a high gloss finish.

Benefits:

  • High gloss surface reduces dray, improves flow and pump efficiency
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion insures reliable performance with no undercutting or under film corrosion
  • Labor and downtime costs are reduced due to ease of application
  • No heat curing required
  • Performs well under fluctuating chemical environments

Suggested Uses:

  • Fans & Housings
  • Heat Exchangers
  • Hoppers
  • Hydropulpers
  • Pump Casings
  • Sand Filter Vessels
  • Structural Steel
  • Tanks and Vessels
  • Volutes
  • Wet Scrubbers
  • Valves
  • Coal Hoppers and Feeders
  • Waterboxes
  • Cooling Water Pumps
  • Wear Plates
  • Coal Screens
  • Impellers
  • Condensers
  • Vacuum Pumps
  • Pitted Tanks and Pipes
  • Pulp Dewatering Screws

Information provided by Chesterton

Vendors:
Available Properties
  • Density, Cured
  • Hardness, Rockwell R, ASTM D785
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength at Break, ASTM D638
  • Flexural Strength, ASTM D790
  • Compressive Strength, ASTM D695
  • CTE, linear, ASTM C531
  • Maximum Service Temperature, Air, Wet Service
  • Maximum Service Temperature, Air, Dry Service
  • Cure Time, Light Load
  • Cure Time, Overend Coat
  • Cure Time, Light Load
  • Cure Time, Full Load
  • Cure Time, Overend Coat
  • Cure Time, Light Load
  • Cure Time, Full Load
  • Cure Time, Full Chemical
  • Cure Time, Overend Coat
  • Cure Time, Light Load
  • Cure Time, Overend Coat
  • Cure Time, Full Load
  • Cure Time, Full Chemical
  • Cure Time, Full Load
  • Cure Time, Full Chemical
  • Cure Time, Full Chemical
  • Tack-Free Time
  • Tack-Free Time
  • Tack-Free Time
  • Tack-Free Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.