Good to excellent corrosion resistance. Excellent cold workability; good hot formability. Applications: trolley wire, heating pads, electric-blanket elements, spring contacts, railbands, high-strength transmission lines, connectors, cable wrap, switch gear components and wave guide cavities. Test specimen: rod - 13mm diameter; hard temper. |
C108, ISO CuCd1, A1/3, cadmium bronze, copper-cadmium |