MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Kolon KOPEL® KP3755 Specialty TPE Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: KOPEL® is a thermoplastic polyester elastomer which is a new engineering rubber having combined properties of conventional rubber and thermoplastic. Its flexibility and elastic recovery are very similar to rubber, but its processability is much superior to rubber. While its flexibility and elastic recovery are similar to rubber, its mechanical properties-heat resistance, weather resistance and UV stability-are far greater than the performance of rubber.

Excellent flexibility and creep resistance, good mechanical properties and heat stability, good chemical resistance

Information provided by US distributor, API-Kolon.

Vendors:
Available Properties
  • Density, ASTM D792, DIN 53479
  • Water Absorption, ASTM D570, DIN 53475
  • Linear Mold Shrinkage, ASTM D955
  • Melt Flow, ASTM D1238
  • Hardness, Shore D, ASTM D2240, DIN 53505
  • Tensile Strength, Ultimate, ASTM D638, DIN 53455
  • Elongation at Break, ASTM D638, DIN 53455
  • Flexural Yield Strength, ASTM D790, DIN 53455
  • Resilience
  • Izod Impact, Notched, ASTM D256, DIN 53453
  • Izod Impact, Notched, Low Temp
  • Taber Abrasion, mg/1000 Cycles, CS-17 WHEEL; ASTM D1044
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648, DIN 53461
  • Brittleness Temperature, Solenoid Brittle Point; ASTM D746
  • Flammability, UL94, per KOLON R&D Center
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic
Thermoplastic Elastomer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.