MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Vycom FLAMETEC™ KYTEC® PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF)

Material Notes: Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when exposed to harsh thermal, chemical, and ultraviolet environments. Kytec has a continuous use temperature of 235º F. Kytec is chemically resistant to most acids, bases, and organic solvents and is ideally suited for handling wet or dry chlorine, bromine and other halogens.

FEATURES AND BENEFITS

  • Weldability- Easy to fabricate and thermoplastically weldable.
  • Strength- Good tensile strength and mechanical abrasion resistance.
  • Purity- An ultra-pure material.
  • Chemical Resistance- Resistance to a broad range of chemistries.
  • Fire Safe- Meets FM4910 criteria and is FM listed.

Information provided by Compression Polymers Corp - Vycom

Vendors:
Available Properties
  • Density, ASTM D792
  • Water Absorption, ASTM D570
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D638
  • Tensile Strength, Yield, ASTM D638
  • Elongation at Break, ASTM D638
  • Elongation at Yield, ASTM D638
  • Tensile Modulus, ASTM D638
  • Flexural Strength, ASTM D790
  • Flexural Modulus, ASTM D790
  • Compressive Strength, ASTM D695
  • Izod Impact, Unnotched, ASTM D256
  • Coefficient of Friction, ASTM D1894
  • Coefficient of Friction, Static, ASTM D1894
  • Volume Resistivity, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Strength, ASTM D149
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Arc Resistance, ASTM D495
  • CTE, linear, ASTM D696
  • Thermal Conductivity, ASTM C177
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Brittleness Temperature, ASTM D2236
  • Oxygen Index, ASTM D2863
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
CPC - Vycom Co. Compression Plastics Corporation

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.