MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Danquinsa MORCHEM UD 5055F Polyurethane dispersion
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: MORCHEM UD 5055F is an aliphatic, aqueous polyurethane dispersion for the production of adhesives and coatings.

Application: MORCHEM UD 5055F is used for the modification of different aqueous polyurethane adhesives, specially to adjust the viscosity. Even mixings with other dispersions are possible. Produced polyurethane adhesives can be vet bonded as onesite-adhesive or as reactivation adhesive, whereby both bonding areas must be striked with the dispersion. The films should be in a dry condition as they must be reactivated later at 70°C. For the crosslinking it can be added 5% of DANCURE 101 or MORCHEM CA-15. After the addition of the hardener it has to pay attention to the potlife of approx. 6 hours

Information provided by Danquinsa GMBH

Vendors:
Available Properties
  • Solids Content
  • pH
  • Viscosity
  • Storage Temperature
  • Hardness, Shore A
  • Tensile Strength, DIN 53.504
  • Elongation at Break, DIN 53.504
  • 100% Modulus, DIN 53.504
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.