Description of Product: This specification covers molybdenum alloy (molybdenum + 0.5% titanium + 0.1% zirconium) pressed and sintered billet. Physical Properties: Density: The as-sintered density will be 94% minimum, based on 10.13 g/cakm³. No defect will exceed a No. 8 FBH as determined by ultrasonic inspection. Dimensional Tolerances: Billet will be in the pressed and sintered condition. A machined surface can also be supplied. Information provided by H.C. Starck. Elmet Technologies Acquired H.C. Starck Solutions Americas in 2023. |