MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Master Bond adhesives
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, make surface milling by the end user superfluous. This combination of properties enables significant cost savings in machining. Applications include reference plates, machine housings, transport tables, jigs, robot arms.

Information provided by manufacturer

Key Words: EN AW-7075 T651
Vendors:
Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Brinell
  • Hardness, Brinell
  • Tensile Strength, Standard EN 485-2, Temper T651
  • Tensile Strength, Standard EN 485-2, Temper T651
  • Tensile Strength, Standard EN 485-2, Temper T651
  • Tensile Strength, Standard EN 485-2, Temper T651
  • Tensile Strength, Standard EN 485-2, Temper T651
  • Tensile Strength, Typical Strength
  • Tensile Strength, Typical Strength
  • Tensile Strength, Typical Strength
  • Tensile Strength, Yield, Standard EN 485-2, Temper T651
  • Tensile Strength, Yield, Standard EN 485-2, Temper T651
  • Tensile Strength, Yield, Standard EN 485-2, Temper T651
  • Tensile Strength, Yield, Standard EN 485-2, Temper T651
  • Tensile Strength, Yield, Typical Strength
  • Tensile Strength, Yield, Standard EN 485-2, Temper T651
  • Tensile Strength, Yield, Typical Strength
  • Tensile Strength, Yield, Typical Strength
  • Elongation at Break, Standard EN 485-2, Temper T651
  • Elongation at Break, Standard EN 485-2, Temper T651
  • Elongation at Break, Standard EN 485-2, Temper T651
  • Elongation at Break, Standard EN 485-2, Temper T651
  • Elongation at Break, Standard EN 485-2, Temper T651
  • Elongation at Break, Typical Elongation
  • Elongation at Break, Typical Elongation
  • Elongation at Break, Typical Elongation
  • Modulus of Elasticity
  • Electrical Resistivity, Temper T651
  • CTE, linear
  • Thermal Conductivity, Temper T651
  • Aluminum, Al, as balance
  • Chromium, Cr
  • Copper, Cu
  • Iron, Fe
  • Magnesium, Mg
  • Manganese, Mn
  • Silicon, Si
  • Zinc, Zn
  • Zr+Ti
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Rulon Bearings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.