90TL is a low viscosity and high capillary action for locking and sealing threaded fasteners and close fittings parts after assembly, also to penetrate and seal metal porosity in moulds and in castings. Medium to high strength locking. Highly resistant to heat, corrosion, vibrations, water, gases, oils, hydrocarbons, and many chemicals. Features and Benefits: - Fluorescent UV Indicator
- Highly Resistant to Heat, Corrosion, Vibrations, Water, Gases, Oils, Hydrocarbons, and Many Chemicals
- Medium to High Strength
- High Capillary Action
Information provided by H.B. Fuller Company |