MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Ensinger PEI
Bostik Ultra-Set® SingleStep™ Hardwood Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Bostik’s Ultra-Set® SingleStep™ is a one-part, trowel applied, tacking, moisture-cure urethane adhesive, moisture vapor and sound reduction membrane. This scientifically formulated adhesive and membrane is very tenacious, has extremely low moisture permeability, and is formulated with Bostik’s patent pending Thickness-Control™ Spacer Technology to ensure proper membrane thickness between hardwood flooring and the substrate. Bostik’s Ultra-Set SingleStep does NOT contain any water, and has zero VOC's as per SCAQMD 1168.

Information provided by Bostik

Vendors:
Available Properties
  • Density
  • Volatile Organic Compounds (VOC) Content, SCAQMD Rule #1168
  • Water Vapor Transmission, ASTM E96
  • Elongation at Break
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Flash Point
  • Processing Temperature, Application
  • Cure Time, Light foot traffic
  • Cure Time, Normal foot traffic
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Proto3000 – 3D Engineering Solutions
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.